Corrosion Time Series Classification using the Continuous Wavelet Transform and MML Density Estimation
Corrosion causes many failures in chemical process installations. These failures generate high costs, therefore an effective corrosion monitoring system obtrudes. This paper focuse...
Gert Van Dijck, M. Wevers, Marc M. Van Hulle