Sciweavers
Explore
Publications
Books
Software
Tutorials
Presentations
Lectures Notes
Datasets
Labs
Conferences
Community
Upcoming
Conferences
Top Ranked Papers
Most Viewed Conferences
Conferences by Acronym
Conferences by Subject
Conferences by Year
Tools
PDF Tools
Image Tools
Text Tools
OCR Tools
Symbol and Emoji Tools
On-screen Keyboard
Latex Math Equation to Image
Smart IPA Phonetic Keyboard
Community
Sciweavers
About
Terms of Use
Privacy Policy
Cookies
230
click to vote
CVPR
2011
IEEE
396
views
Computer Vision
»
more
CVPR 2011
»
A Multichannel Edge-Weighted Centroidal Voronoi Tessellation Algorithm for 3D Superalloy Image Segmentation
15 years 3 months ago
Download
www.cse.sc.edu
In material science and engineering, the grain structure inside a super-alloy sample determines its mechanical and physical properties. In this paper, we develop a new Multichannel...
Y. Cao, L. Ju, Q. Zou, C. Qu, S. Wang